General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.3 - 8.8 g/cm³ Show Material materials with Densidad of 8.3 - 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 1.27 - 12.7 mm Show Material materials with Diámetro of 1.27 - 12.7 mm |
Diámetro exterior | 9.5 - 76 mm Show Material materials with Diámetro exterior of 9.5 - 76 mm |
Wall thickness | 10-20% of outside diameter |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell B | 23.0 °C | 45 - 85 [-] Show Material materials with Dureza Rockwell B of 45 - 85 [-] | |
Elongación | 23.0 °C | 1 - 60 % Show Material materials with Elongación of 1 - 60 % | min.,min., for wire with 0.1mm diameter and more. |
Límite elástico | 23.0 °C | 1220 MPa Show Material materials with Límite elástico of 1220 MPa | |
Límite elástico Rp 0,2 | 23.0 °C | 130 - 1520 MPa Show Material materials with Límite elástico Rp 0,2 of 130 - 1520 MPa | |
Módulo elástico | 23.0 °C | 130 - 131 GPa Show Material materials with Módulo elástico of 130 - 131 GPa | |
Resistencia a la tracción | 23.0 °C | 410 - 1590 MPa Show Material materials with Resistencia a la tracción of 410 - 1590 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 360 J/(kg·K) Show Material materials with Calor específico of 360 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.75E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.75E-5 - 1.8E-5 1/K |
Conductividad térmica | 23.0 °C | 105 - 110 W/(m·K) Show Material materials with Conductividad térmica of 105 - 110 W/(m·K) |
Temperatura de fusión | 870 °C Show Material materials with Temperatura de fusión of 870 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 5.8E-6 - 7.8E-6 Ω·m Show Material materials with Resistividad eléctrica of 5.8E-6 - 7.8E-6 Ω·m |
Specific Electrical conductivity | 22 - 30 % IACS Show Material materials with Specific Electrical conductivity of 22 - 30 % IACS |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Material materials with Permeabilidad magnética relativa of 1 [-] | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0 - 0.2 % Show Material materials with Aluminio of 0 - 0.2 % | |
Berilio | 1.8 - 2 % Show Material materials with Berilio of 1.8 - 2 % | |
Cobalto | 0.2 % Show Material materials with Cobalto of 0.2 % | min. Nickel + Cobalt |
Cobre | 96.1 - 98 % Show Material materials with Cobre of 96.1 - 98 % | Balance |
Hierro | 0 - 0.6 % Show Material materials with Hierro of 0 - 0.6 % | max., Nickel + Cobalt + Iron,max. Nickel + Cobalt + Iron |
Níquel | 0.2 - 0.6 % Show Material materials with Níquel of 0.2 - 0.6 % | min. Nickel + Cobalt |
Otro | 0 - 0.5 % Show Material materials with Otro of 0 - 0.5 % | |
Plomo | 0.2 - 0.6 % Show Material materials with Plomo of 0.2 - 0.6 % | |
Silicona | 0 - 0.2 % Show Material materials with Silicona of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include bushings and bearings for aircraft as well as drill collars and instrument housings for oil and gas exploration.,Typical applications for parts finished by forging or extrusion of these alloys include undersea instrument and repeater housings, generator rings, and resistance welding components.,Typical applications include precision coil springs and pins for burn-in and test socket contacts and probe pins, computer processor socket contacts, cold headed fasteners, modular jack contacts, woven mesh electromagnetic shielding gaskets and resilient eyeglass frames.,EtchMet alloy is a material that is tailor made for the springs in voice coil motors and optical image stabilization systems common in smart phone cameras. |