General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.75 - 8.9 g/cm³ Show Material materials with Densidad of 8.75 - 8.9 g/cm³ |
Medidas
Property | Value | Comment | |
---|---|---|---|
Ancho | 1.27 - 559 mm Show Material materials with Ancho of 1.27 - 559 mm | ||
Diámetro | 1.27 - 12.7 mm Show Material materials with Diámetro of 1.27 - 12.7 mm | ||
Diámetro exterior | 0.76 - 76 mm Show Material materials with Diámetro exterior of 0.76 - 76 mm | Rod | |
Espesor | 0.05 - 76 mm Show Material materials with Espesor of 0.05 - 76 mm | Bar | |
Longitud | 610 - 91000 mm Show Material materials with Longitud of 610 - 91000 mm | max. Rod and Bar | |
Wall thickness | Typically 10 to 20% of OD |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell C | 23.0 °C | 18 - 26 [-] Show Material materials with Dureza Rockwell C of 18 - 26 [-] | |
Dureza Vickers | 23.0 °C | 216 - 287 [-] Show Material materials with Dureza Vickers of 216 - 287 [-] | |
Elongación | 23.0 °C | 5 - 25 % Show Material materials with Elongación of 5 - 25 % | for strip with 0.1mm and thicker.,min. |
Límite elástico Rp 0,2 | 23.0 °C | 650 - 900 MPa Show Material materials with Límite elástico Rp 0,2 of 650 - 900 MPa | |
Módulo de cizallamiento | 23.0 °C | 52 GPa Show Material materials with Módulo de cizallamiento of 52 GPa | |
Módulo elástico | 23.0 °C | 120 - 138 GPa Show Material materials with Módulo elástico of 120 - 138 GPa | |
Plegabilidad 90 ° bidireccional | 23.0 °C | 2 [-] Show Material materials with Plegabilidad 90 ° bidireccional of 2 [-] | for strip with 0.25mm and thinner. |
Plegabilidad 90 ° en peso bruto | 23.0 °C | 1 [-] Show Material materials with Plegabilidad 90 ° en peso bruto of 1 [-] | for strip with 0.25mm and thinner. |
Resistencia a la tracción | 23.0 °C | 750 - 970 MPa Show Material materials with Resistencia a la tracción of 750 - 970 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 390 J/(kg·K) Show Material materials with Calor específico of 390 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.76E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.76E-5 1/K |
Conductividad térmica | 23.0 °C | 167 - 260 W/(m·K) Show Material materials with Conductividad térmica of 167 - 260 W/(m·K) |
Temperatura de fusión | 1030 - 1040 °C Show Material materials with Temperatura de fusión of 1030 - 1040 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 3.8E-8 - 3.8E-6 Ω·m Show Material materials with Resistividad eléctrica of 3.8E-8 - 3.8E-6 Ω·m |
Specific Electrical conductivity | 45 - 60 % IACS Show Material materials with Specific Electrical conductivity of 45 - 60 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0 - 0.2 % Show Material materials with Aluminio of 0 - 0.2 % | |
Berilio | 0.2 - 0.6 % Show Material materials with Berilio of 0.2 - 0.6 % | |
Cobalto | 0 - 0.3 % Show Material materials with Cobalto of 0 - 0.3 % | |
Cobre | 95.9 - 98.4 % Show Material materials with Cobre of 95.9 - 98.4 % | Balance |
Hierro | 0 - 0.1 % Show Material materials with Hierro of 0 - 0.1 % | |
Níquel | 1.4 - 2.2 % Show Material materials with Níquel of 1.4 - 2.2 % | |
Otro | 0 - 0.5 % Show Material materials with Otro of 0 - 0.5 % | |
Silicona | 0 - 0.2 % Show Material materials with Silicona of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include high reliability spring contacts for switches and relays.,Aerospace: Landing gear, bearing bushes and high performance fasteners;Automotive: Valve guides, bushes and valve seats;Offshore & marine: Offshore drilling and instrumentation equipment, downhole tooling, valve, pump and shaft components;Other: Deep drawing tooling, plastic moulding dies, tools and plungers, die-casting plunger tips, non-magnetic and non sparking tools, electrical and electronic connectors, springs, fasteners, switchgear, resistance welding electrodes and equipment, flash butt welding dies and inserts, seam welding electrode shafts,Typical applications include resistance welding components, and inserts for metal die casting, injection molding and blow molding.,Typical applications include dies casting plunger tips and dies for steel extrusion.,Typical applications include heat exchanger tubing and resistance welding components.,Typical applications include coil springs and formed wire contacts. | |
Corrosion properties | High corrosion resistance | |
General machinability | Very good machinability |