General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.36 - 8.8 g/cm³ Show Material materials with Densidad of 8.36 - 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 1.27 - 12.7 mm Show Material materials with Diámetro of 1.27 - 12.7 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 2 - 25 % Show Material materials with Elongación of 2 - 25 % |
Límite elástico | 23.0 °C | 1050 MPa Show Material materials with Límite elástico of 1050 MPa |
Límite elástico Rp 0,2 | 23.0 °C | 510 - 730 MPa Show Material materials with Límite elástico Rp 0,2 of 510 - 730 MPa |
Módulo elástico | 23.0 °C | 130 - 131 GPa Show Material materials with Módulo elástico of 130 - 131 GPa |
Resistencia a la tracción | 23.0 °C | 620 - 1140 MPa Show Material materials with Resistencia a la tracción of 620 - 1140 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 360 J/(kg·K) Show Material materials with Calor específico of 360 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.75E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.75E-5 - 1.8E-5 1/K |
Conductividad térmica | 23.0 °C | 105 - 110 W/(m·K) Show Material materials with Conductividad térmica of 105 - 110 W/(m·K) |
Temperatura de fusión | 870 °C Show Material materials with Temperatura de fusión of 870 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 6.2E-6 - 7.8E-6 Ω·m Show Material materials with Resistividad eléctrica of 6.2E-6 - 7.8E-6 Ω·m |
Specific Electrical conductivity | 22 - 28 % IACS Show Material materials with Specific Electrical conductivity of 22 - 28 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0 - 0.2 % Show Material materials with Aluminio of 0 - 0.2 % | |
Berilio | 1.8 - 2 % Show Material materials with Berilio of 1.8 - 2 % | |
Cobalto | 0.2 % Show Material materials with Cobalto of 0.2 % | min. Nickel + Cobalt |
Cobre | 96.1 - 98 % Show Material materials with Cobre of 96.1 - 98 % | Balance |
Hierro | 0 - 0.6 % Show Material materials with Hierro of 0 - 0.6 % | max., Nickel + Cobalt + Iron |
Níquel | 0.2 - 0.6 % Show Material materials with Níquel of 0.2 - 0.6 % | min. Nickel + Cobalt |
Otro | 0 - 0.5 % Show Material materials with Otro of 0 - 0.5 % | |
Silicona | 0 - 0.2 % Show Material materials with Silicona of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include precision coil springs and pins for burn-in and test socket contacts and probe pins, computer processor socket contacts, cold headed fasteners, modular jack contacts, woven mesh electromagnetic shielding gaskets and resilient eyeglass frames. |