General
Property | Value | Condition |
---|---|---|
Densidad | 4.5 g/cm³ Show Material materials with Densidad of 4.5 g/cm³ | Transformed-Beta |
Mecánica
Property | Value | Condition |
---|---|---|
Elongación | 6.9 % Show Material materials with Elongación of 6.9 % | Transformed-Beta |
Límite elástico | 870.0 MPa Show Material materials with Límite elástico of 870.0 MPa | Transformed-Beta |
Módulo elástico | 110.0 GPa Show Material materials with Módulo elástico of 110.0 GPa | Transformed-Beta |
Resistencia a la tracción | 950.0 MPa Show Material materials with Resistencia a la tracción of 950.0 MPa | Transformed-Beta |
Aplicaciones térmicas
Property | Value | Condition | Comment |
---|---|---|---|
Calor específico | 570.0 J/(kg·K) Show Material materials with Calor específico of 570.0 J/(kg·K) | Transformed-Beta | |
Coeficiente de dilatación térmica | 9.5e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 9.5e-06 1/K | Transformed-Beta | |
Conductividad térmica | 7.3 W/(m·K) Show Material materials with Conductividad térmica of 7.3 W/(m·K) | Transformed-Beta | |
Temperatura de fusión | 1500.0 - 1750.0 °C Show Material materials with Temperatura de fusión of 1500.0 - 1750.0 °C | Typical for Titanium Alpha Beta Alloy |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 5.5 - 6.5 % Show Material materials with Aluminio of 5.5 - 6.5 % | Transformed-Beta |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % | Transformed-Beta |
Hidrógeno | 0.015 % Show Material materials with Hidrógeno of 0.015 % | Transformed-Beta |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % | Transformed-Beta |
Nitrógeno | 0.03 % Show Material materials with Nitrógeno of 0.03 % | Transformed-Beta |
Otro | 0.4 % Show Material materials with Otro of 0.4 % | Transformed-Beta |
Oxígeno | 0.13 % Show Material materials with Oxígeno of 0.13 % | Transformed-Beta |
Rutenio | 0.08 - 0.14 % Show Material materials with Rutenio of 0.08 - 0.14 % | Transformed-Beta |
Titanio | 88.0 - 90.9 % Show Material materials with Titanio of 88.0 - 90.9 % | Transformed-Beta |
Vanadio | 3.5 - 4.5 % Show Material materials with Vanadio of 3.5 - 4.5 % | Transformed-Beta |