General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.2 g/cm³ Show Material materials with Densidad of 8.2 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Maraging Steel |
Elongación | 23.0 °C | 9 % Show Material materials with Elongación of 9 % | |
Límite elástico | 23.0 °C | 2100 MPa Show Material materials with Límite elástico of 2100 MPa | |
Módulo elástico | 23.0 °C | 190 GPa Show Material materials with Módulo elástico of 190 GPa | |
Resistencia a la tracción | 23.0 °C | 2030 MPa Show Material materials with Resistencia a la tracción of 2030 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K | |
Conductividad térmica | 23.0 °C | 20 - 25 W/(m·K) Show Material materials with Conductividad térmica of 20 - 25 W/(m·K) | Typical for Maraging Steel |
Temperatura de fusión | 1425 - 1505 °C Show Material materials with Temperatura de fusión of 1425 - 1505 °C | Typical for Maraging Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 - 0.15 % Show Material materials with Aluminio of 0.05 - 0.15 % |
Azufre | 0 - 0.01 % Show Material materials with Azufre of 0 - 0.01 % |
Boro | 0 - 3E-3 % Show Material materials with Boro of 0 - 3E-3 % |
Calcio | 0 - 0.05 % Show Material materials with Calcio of 0 - 0.05 % |
Carbono | 0 - 0.03 % Show Material materials with Carbono of 0 - 0.03 % |
Circonio | 0 - 0.02 % Show Material materials with Circonio of 0 - 0.02 % |
Cobalto | 8.5 - 9.5 % Show Material materials with Cobalto of 8.5 - 9.5 % |
Fósforo | 0 - 0.01 % Show Material materials with Fósforo of 0 - 0.01 % |
Hierro | 65 - 68.4 % Show Material materials with Hierro of 65 - 68.4 % |
Manganeso | 0 - 0.1 % Show Material materials with Manganeso of 0 - 0.1 % |
Molibdeno | 4.6 - 5.2 % Show Material materials with Molibdeno of 4.6 - 5.2 % |
Níquel | 18 - 19 % Show Material materials with Níquel of 18 - 19 % |
Silicona | 0 - 0.1 % Show Material materials with Silicona of 0 - 0.1 % |
Titanio | 0.5 - 0.8 % Show Material materials with Titanio of 0.5 - 0.8 % |