General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.7 g/cm³ Show Material materials with Densidad of 7.7 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Elongación | 23.0 °C | 18 % Show Material materials with Elongación of 18 % | |
Límite elástico | 23.0 °C | 430 MPa Show Material materials with Límite elástico of 430 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Martensitic Stainless Steel |
Módulo elástico | 23.0 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa | |
Resistencia a la tracción | 23.0 °C | 740 MPa Show Material materials with Resistencia a la tracción of 740 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 430 J/(kg·K) Show Material materials with Calor específico of 430 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 1/K |
Conductividad térmica | 23.0 °C | 15 W/(m·K) Show Material materials with Conductividad térmica of 15 W/(m·K) |
Temperatura de fusión | 1370 °C Show Material materials with Temperatura de fusión of 1370 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.015 % Show Material materials with Azufre of 0 - 0.015 % |
Carbono | 0.75 - 1 % Show Material materials with Carbono of 0.75 - 1 % |
Cromo | 16 - 19 % Show Material materials with Cromo of 16 - 19 % |
Fósforo | 0 - 0.04 % Show Material materials with Fósforo of 0 - 0.04 % |
Hierro | 76.6 - 83.3 % Show Material materials with Hierro of 76.6 - 83.3 % |
Manganeso | 0 - 1 % Show Material materials with Manganeso of 0 - 1 % |
Molibdeno | 0 - 1.3 % Show Material materials with Molibdeno of 0 - 1.3 % |
Silicona | 0 - 1 % Show Material materials with Silicona of 0 - 1 % |
Vanadio | 0.07 - 0.12 % Show Material materials with Vanadio of 0.07 - 0.12 % |