General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Duplex Stainless Steel |
Elongación | 23.0 °C | 23 % Show Material materials with Elongación of 23 % | |
Límite elástico | 23.0 °C | 630 MPa Show Material materials with Límite elástico of 630 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Duplex Stainless Steel |
Módulo elástico | 23.0 °C | 200 GPa Show Material materials with Módulo elástico of 200 GPa | |
Resistencia a la tracción | 23.0 °C | 870 MPa Show Material materials with Resistencia a la tracción of 870 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K | |
Conductividad térmica | 23.0 °C | 15 W/(m·K) Show Material materials with Conductividad térmica of 15 W/(m·K) | |
Temperatura de fusión | 1375 - 1450 °C Show Material materials with Temperatura de fusión of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Temperatura máx. de funcionamiento | 300 °C Show Material materials with Temperatura máx. de funcionamiento of 300 °C | Typical for Duplex Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.03 % Show Material materials with Azufre of 0 - 0.03 % |
Carbono | 0 - 0.04 % Show Material materials with Carbono of 0 - 0.04 % |
Cobre | 1 - 2.5 % Show Material materials with Cobre of 1 - 2.5 % |
Cromo | 24 - 27 % Show Material materials with Cromo of 24 - 27 % |
Fósforo | 0 - 0.04 % Show Material materials with Fósforo of 0 - 0.04 % |
Hierro | 56.4 - 67 % Show Material materials with Hierro of 56.4 - 67 % |
Manganeso | 0 - 2 % Show Material materials with Manganeso of 0 - 2 % |
Molibdeno | 2.9 - 4 % Show Material materials with Molibdeno of 2.9 - 4 % |
Nitrógeno | 0.1 - 0.3 % Show Material materials with Nitrógeno of 0.1 - 0.3 % |
Níquel | 4.5 - 8 % Show Material materials with Níquel of 4.5 - 8 % |
Silicona | 0 - 1 % Show Material materials with Silicona of 0 - 1 % |