General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.1 g/cm³ Show Material materials with Densidad of 8.1 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 23.0 °C | 46 % Show Material materials with Elongación of 46 % | |
Límite elástico | 23.0 °C | 490 MPa Show Material materials with Límite elástico of 490 MPa | |
Módulo elástico | 23.0 °C | 190 GPa Show Material materials with Módulo elástico of 190 GPa | |
Resistencia a la tracción | 23.0 °C | 860 MPa Show Material materials with Resistencia a la tracción of 860 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K |
Conductividad térmica | 23.0 °C | 8.6 W/(m·K) Show Material materials with Conductividad térmica of 8.6 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 5E-3 % Show Material materials with Azufre of 0 - 5E-3 % |
Carbono | 0 - 0.02 % Show Material materials with Carbono of 0 - 0.02 % |
Cobre | 0.3 - 0.6 % Show Material materials with Cobre of 0.3 - 0.6 % |
Cromo | 23 - 25 % Show Material materials with Cromo of 23 - 25 % |
Fósforo | 0 - 0.03 % Show Material materials with Fósforo of 0 - 0.03 % |
Hierro | 38.3 - 46.3 % Show Material materials with Hierro of 38.3 - 46.3 % |
Manganeso | 2 - 4 % Show Material materials with Manganeso of 2 - 4 % |
Molibdeno | 7 - 8 % Show Material materials with Molibdeno of 7 - 8 % |
Nitrógeno | 0.45 - 0.55 % Show Material materials with Nitrógeno of 0.45 - 0.55 % |
Níquel | 21 - 23 % Show Material materials with Níquel of 21 - 23 % |
Silicona | 0 - 0.5 % Show Material materials with Silicona of 0 - 0.5 % |