General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 1.9 g/cm³ Show Material materials with Densidad of 1.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Magnesium |
Elongación | 23.0 °C | 13 % Show Material materials with Elongación of 13 % | |
Límite elástico | 23.0 °C | 130 MPa Show Material materials with Límite elástico of 130 MPa | |
Módulo de cizallamiento | 23.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | Typical for Magnesium |
Módulo elástico | 23.0 °C | 45 GPa Show Material materials with Módulo elástico of 45 GPa | |
Resistencia a la tracción | 23.0 °C | 240 MPa Show Material materials with Resistencia a la tracción of 240 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 1040 J/(kg·K) Show Material materials with Calor específico of 1040 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.6E-5 1/K |
Conductividad térmica | 23.0 °C | 72 W/(m·K) Show Material materials with Conductividad térmica of 72 W/(m·K) |
Temperatura de fusión | 600 °C Show Material materials with Temperatura de fusión of 600 °C |
Chemical properties
Property | Value |
---|---|
Aluminio | 2.4 - 3.6 % Show Material materials with Aluminio of 2.4 - 3.6 % |
Calcio | 0 - 0.04 % Show Material materials with Calcio of 0 - 0.04 % |
Cobre | 0 - 0.05 % Show Material materials with Cobre of 0 - 0.05 % |
Hierro | 0 - 0.05 % Show Material materials with Hierro of 0 - 0.05 % |
Magnesio | 93.6 - 97.1 % Show Material materials with Magnesio of 93.6 - 97.1 % |
Manganeso | 0.05 - 1 % Show Material materials with Manganeso of 0.05 - 1 % |
Níquel | 0 - 5E-3 % Show Material materials with Níquel of 0 - 5E-3 % |
Otro | 0 - 0.3 % Show Material materials with Otro of 0 - 0.3 % |
Silicona | 0 - 0.1 % Show Material materials with Silicona of 0 - 0.1 % |
Zinc | 0.5 - 1.5 % Show Material materials with Zinc of 0.5 - 1.5 % |