General
Property | Value | Condition |
---|---|---|
Densidad | 4.5 g/cm³ Show Material materials with Densidad of 4.5 g/cm³ | Cold Worked And Stress Relieved |
Mecánica
Property | Value | Condition |
---|---|---|
Elongación | 12.0 % Show Material materials with Elongación of 12.0 % | Cold Worked And Stress Relieved |
Límite elástico | 830.0 MPa Show Material materials with Límite elástico of 830.0 MPa | Cold Worked And Stress Relieved |
Módulo elástico | 110.0 GPa Show Material materials with Módulo elástico of 110.0 GPa | Cold Worked And Stress Relieved |
Resistencia a la tracción | 990.0 MPa Show Material materials with Resistencia a la tracción of 990.0 MPa | Cold Worked And Stress Relieved |
Aplicaciones térmicas
Property | Value | Condition | Comment |
---|---|---|---|
Calor específico | 490.0 J/(kg·K) Show Material materials with Calor específico of 490.0 J/(kg·K) | Cold Worked And Stress Relieved | |
Coeficiente de dilatación térmica | 9.1e-06 1/K Show Material materials with Coeficiente de dilatación térmica of 9.1e-06 1/K | Cold Worked And Stress Relieved | |
Conductividad térmica | 8.1 W/(m·K) Show Material materials with Conductividad térmica of 8.1 W/(m·K) | Cold Worked And Stress Relieved | |
Temperatura de fusión | 1668.0 °C Show Material materials with Temperatura de fusión of 1668.0 °C | Typical for Titanium |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 2.5 - 3.5 % Show Material materials with Aluminio of 2.5 - 3.5 % | Cold Worked And Stress Relieved |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % | Cold Worked And Stress Relieved |
Hidrógeno | 0.015 % Show Material materials with Hidrógeno of 0.015 % | Cold Worked And Stress Relieved |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % | Cold Worked And Stress Relieved |
Nitrógeno | 0.03 % Show Material materials with Nitrógeno of 0.03 % | Cold Worked And Stress Relieved |
Otro | 0.4 % Show Material materials with Otro of 0.4 % | Cold Worked And Stress Relieved |
Oxígeno | 0.15 % Show Material materials with Oxígeno of 0.15 % | Cold Worked And Stress Relieved |
Titanio | 92.6 - 95.5 % Show Material materials with Titanio of 92.6 - 95.5 % | Cold Worked And Stress Relieved |
Vanadio | 2.0 - 3.0 % Show Material materials with Vanadio of 2.0 - 3.0 % | Cold Worked And Stress Relieved |