General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 5 g/cm³ Show Material materials with Densidad of 5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Zinc Aluminium |
Elongación | 23.0 °C | 2 % Show Material materials with Elongación of 2 % | |
Límite elástico | 23.0 °C | 370 MPa Show Material materials with Límite elástico of 370 MPa | |
Módulo elástico | 23.0 °C | 78 GPa Show Material materials with Módulo elástico of 78 GPa | |
Resistencia a la tracción | 23.0 °C | 430 MPa Show Material materials with Resistencia a la tracción of 430 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 530 J/(kg·K) Show Material materials with Calor específico of 530 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.6E-5 1/K |
Conductividad térmica | 23.0 °C | 130 W/(m·K) Show Material materials with Conductividad térmica of 130 W/(m·K) |
Temperatura de fusión | 380 °C Show Material materials with Temperatura de fusión of 380 °C |
Chemical properties
Property | Value |
---|---|
Aluminio | 25 - 28 % Show Material materials with Aluminio of 25 - 28 % |
Cadmio | 0 - 6E-3 % Show Material materials with Cadmio of 0 - 6E-3 % |
Cobre | 2 - 2.5 % Show Material materials with Cobre of 2 - 2.5 % |
Estaño | 0 - 3E-3 % Show Material materials with Estaño of 0 - 3E-3 % |
Hierro | 0 - 0.1 % Show Material materials with Hierro of 0 - 0.1 % |
Magnesio | 0.01 - 0.02 % Show Material materials with Magnesio of 0.01 - 0.02 % |
Níquel | 0 - 0.02 % Show Material materials with Níquel of 0 - 0.02 % |
Plomo | 0 - 6E-3 % Show Material materials with Plomo of 0 - 6E-3 % |
Silicona | 0 - 0.08 % Show Material materials with Silicona of 0 - 0.08 % |
Zinc | 69.3 - 73 % Show Material materials with Zinc of 69.3 - 73 % |