General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.7 g/cm³ Show Material materials with Densidad of 8.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 34 - 35 % Show Material materials with Elongación of 34 - 35 % |
Límite elástico | 23.0 °C | 330 - 460 MPa Show Material materials with Límite elástico of 330 - 460 MPa |
Módulo elástico | 23.0 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa |
Resistencia a la tracción | 23.0 °C | 810 - 920 MPa Show Material materials with Resistencia a la tracción of 810 - 920 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K |
Conductividad térmica | 23.0 °C | 12 W/(m·K) Show Material materials with Conductividad térmica of 12 W/(m·K) |
Temperatura de fusión | 1290 °C Show Material materials with Temperatura de fusión of 1290 °C |
Chemical properties
Property | Value |
---|---|
Aluminio | 0 - 0.4 % Show Material materials with Aluminio of 0 - 0.4 % |
Azufre | 0 - 0.015 % Show Material materials with Azufre of 0 - 0.015 % |
Carbono | 0 - 0.1 % Show Material materials with Carbono of 0 - 0.1 % |
Cobalto | 0 - 1 % Show Material materials with Cobalto of 0 - 1 % |
Cromo | 20 - 23 % Show Material materials with Cromo of 20 - 23 % |
Fósforo | 0 - 0.02 % Show Material materials with Fósforo of 0 - 0.02 % |
Hierro | 0 - 5 % Show Material materials with Hierro of 0 - 5 % |
Manganeso | 0 - 0.5 % Show Material materials with Manganeso of 0 - 0.5 % |
Molibdeno | 8 - 10 % Show Material materials with Molibdeno of 8 - 10 % |
Niobio | 3.2 - 4.2 % Show Material materials with Niobio of 3.2 - 4.2 % |
Níquel | 58 - 68.9 % Show Material materials with Níquel of 58 - 68.9 % |
Silicona | 0 - 0.5 % Show Material materials with Silicona of 0 - 0.5 % |
Titanio | 0 - 0.4 % Show Material materials with Titanio of 0 - 0.4 % |