General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.9 g/cm³ Show Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 23.0 °C | 9.2 - 12 % Show Material materials with Elongación of 9.2 - 12 % | |
Límite elástico | 23.0 °C | 1470 - 1740 MPa Show Material materials with Límite elástico of 1470 - 1740 MPa | |
Módulo elástico | 23.0 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa | |
Resistencia a la tracción | 23.0 °C | 1630 - 1860 MPa Show Material materials with Resistencia a la tracción of 1630 - 1860 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 450 J/(kg·K) Show Material materials with Calor específico of 450 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.03 % Show Material materials with Azufre of 0 - 0.03 % |
Carbono | 0 - 0.05 % Show Material materials with Carbono of 0 - 0.05 % |
Cobre | 1.5 - 2.5 % Show Material materials with Cobre of 1.5 - 2.5 % |
Cromo | 11 - 12.5 % Show Material materials with Cromo of 11 - 12.5 % |
Fósforo | 0 - 0.04 % Show Material materials with Fósforo of 0 - 0.04 % |
Hierro | 71.5 - 79.2 % Show Material materials with Hierro of 71.5 - 79.2 % |
Manganeso | 0 - 0.5 % Show Material materials with Manganeso of 0 - 0.5 % |
Molibdeno | 0 - 0.5 % Show Material materials with Molibdeno of 0 - 0.5 % |
Niobio | 0 - 0.5 % Show Material materials with Niobio of 0 - 0.5 % |
Níquel | 7.5 - 9.5 % Show Material materials with Níquel of 7.5 - 9.5 % |
Silicona | 0 - 0.5 % Show Material materials with Silicona of 0 - 0.5 % |
Titanio | 0.8 - 1.4 % Show Material materials with Titanio of 0.8 - 1.4 % |
Tántalo | 0 - 0.5 % Show Material materials with Tántalo of 0 - 0.5 % |