General
Property | Value | Condition |
---|---|---|
Densidad | 5.4 g/cm³ Show Material materials with Densidad of 5.4 g/cm³ | High Strength |
Mecánica
Property | Value | Condition |
---|---|---|
Elongación | 9.2 % Show Material materials with Elongación of 9.2 % | High Strength |
Límite elástico | 1180.0 MPa Show Material materials with Límite elástico of 1180.0 MPa | High Strength |
Módulo elástico | 150.0 GPa Show Material materials with Módulo elástico of 150.0 GPa | High Strength |
Resistencia a la tracción | 1350.0 MPa Show Material materials with Resistencia a la tracción of 1350.0 MPa | High Strength |
Aplicaciones térmicas
Property | Value | Condition | Comment |
---|---|---|---|
Calor específico | 500.0 J/(kg·K) Show Material materials with Calor específico of 500.0 J/(kg·K) | High Strength | |
Coeficiente de dilatación térmica | 1.1e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1e-05 1/K | High Strength | |
Conductividad térmica | 6.0 - 11.0 W/(m·K) Show Material materials with Conductividad térmica of 6.0 - 11.0 W/(m·K) | Typical for Titanium Beta Alloy | |
Temperatura de fusión | 1550.0 - 1815.0 °C Show Material materials with Temperatura de fusión of 1550.0 - 1815.0 °C | Typical for Titanium Beta Alloy |
Chemical properties
Property | Value | Condition |
---|---|---|
Aluminio | 2.5 - 3.5 % Show Material materials with Aluminio of 2.5 - 3.5 % | High Strength |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % | High Strength |
Hidrógeno | 0.015 % Show Material materials with Hidrógeno of 0.015 % | High Strength |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % | High Strength |
Molibdeno | 14.0 - 16.0 % Show Material materials with Molibdeno of 14.0 - 16.0 % | High Strength |
Niobio | 2.2 - 3.2 % Show Material materials with Niobio of 2.2 - 3.2 % | High Strength |
Nitrógeno | 0.03 % Show Material materials with Nitrógeno of 0.03 % | High Strength |
Otro | 0.4 % Show Material materials with Otro of 0.4 % | High Strength |
Oxígeno | 0.17 % Show Material materials with Oxígeno of 0.17 % | High Strength |
Silicona | 0.15 - 0.25 % Show Material materials with Silicona of 0.15 - 0.25 % | High Strength |
Titanio | 76.0 - 81.2 % Show Material materials with Titanio of 76.0 - 81.2 % | High Strength |