General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 12 % Show Material materials with Elongación of 12 % |
Límite elástico | 23.0 °C | 840 MPa Show Material materials with Límite elástico of 840 MPa |
Módulo elástico | 23.0 °C | 250 GPa Show Material materials with Módulo elástico of 250 GPa |
Resistencia a la tracción | 23.0 °C | 1280 MPa Show Material materials with Resistencia a la tracción of 1280 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 450 J/(kg·K) Show Material materials with Calor específico of 450 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K |
Conductividad térmica | 23.0 °C | 13 W/(m·K) Show Material materials with Conductividad térmica of 13 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminio | 0 - 0.1 % Show Material materials with Aluminio of 0 - 0.1 % |
Azufre | 0 - 0.01 % Show Material materials with Azufre of 0 - 0.01 % |
Boro | 0 - 0.01 % Show Material materials with Boro of 0 - 0.01 % |
Carbono | 0 - 0.35 % Show Material materials with Carbono of 0 - 0.35 % |
Cobalto | 58.7 - 68 % Show Material materials with Cobalto of 58.7 - 68 % |
Cromo | 27 - 30 % Show Material materials with Cromo of 27 - 30 % |
Fósforo | 0 - 0.02 % Show Material materials with Fósforo of 0 - 0.02 % |
Hierro | 0 - 0.75 % Show Material materials with Hierro of 0 - 0.75 % |
Manganeso | 0 - 1 % Show Material materials with Manganeso of 0 - 1 % |
Molibdeno | 5 - 7 % Show Material materials with Molibdeno of 5 - 7 % |
Nitrógeno | 0 - 0.25 % Show Material materials with Nitrógeno of 0 - 0.25 % |
Níquel | 0 - 0.5 % Show Material materials with Níquel of 0 - 0.5 % |
Silicona | 0 - 1 % Show Material materials with Silicona of 0 - 1 % |
Titanio | 0 - 0.1 % Show Material materials with Titanio of 0 - 0.1 % |
Wolframio | 0 - 0.2 % Show Material materials with Wolframio of 0 - 0.2 % |