Medidas
Property | Value |
---|---|
Dimensions | Briquette size: 18 x 12 x 7 mm approx. (0.75 x 0.5 x 0.25 inches approx.), pillow shaped |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 3E-3 % Show Supplier Material materials with Azufre of 3E-3 % | max | |
Carbono | 5E-3 % Show Supplier Material materials with Carbono of 5E-3 % | max | |
Nitrógeno | 0.01 % Show Supplier Material materials with Nitrógeno of 0.01 % | max | |
Otro | 0.01 % Show Supplier Material materials with Otro of 0.01 % | total metallic impurities max. | |
Oxígeno | 0.06 % Show Supplier Material materials with Oxígeno of 0.06 % | max | |
Renio | balance |
Technological properties
Property | ||
---|---|---|
Application areas | Common uses: As an addition to superalloys for components in high temperature sectors of aerospace and power generation turbines | |
Processing history | Produced by sintering rhenium metal powder |