General
Property | Value | Comment |
---|---|---|
Rango de tamaño de partículas | 3.5 - 4 µm Show Supplier Material materials with Rango de tamaño de partículas of 3.5 - 4 µm | Fisher S.S.S. (typical value, others as requested) |
Tamaño de partícula | 63000 nm Show Supplier Material materials with Tamaño de partícula of 63000 nm | Sieve analysis from 270 mesh to 100 mesh (typical max value, others as requested) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 3E-3 % Show Supplier Material materials with Azufre of 3E-3 % | max | |
Carbono | 5E-3 % Show Supplier Material materials with Carbono of 5E-3 % | max | |
Nitrógeno | 0.01 % Show Supplier Material materials with Nitrógeno of 0.01 % | max | |
Otro | 0.02 % Show Supplier Material materials with Otro of 0.02 % | total metallic impurities max. | |
Oxígeno | 0.25 % Show Supplier Material materials with Oxígeno of 0.25 % | max | |
Renio | balance |
Technological properties
Property | ||
---|---|---|
Application areas | Common uses: As an alloy addition in superalloys; production of sheet foil, strip or wire for various industrial applications | |
Processing history | Produced by hydrogen reduction of Ammonium Perrhenate |