Chemical properties
Property | Value |
---|---|
Aluminio | 99.98 % Show Supplier Material materials with Aluminio of 99.98 % |
Cobre | 0.0001 % Show Supplier Material materials with Cobre of 0.0001 % |
Cromo | 0.0007 % Show Supplier Material materials with Cromo of 0.0007 % |
Galio | 0.0036 % Show Supplier Material materials with Galio of 0.0036 % |
Hierro | 0.0046 % Show Supplier Material materials with Hierro of 0.0046 % |
Magnesio | 0.0005 % Show Supplier Material materials with Magnesio of 0.0005 % |
Manganeso | 0.0012 % Show Supplier Material materials with Manganeso of 0.0012 % |
Níquel | 0.001 % Show Supplier Material materials with Níquel of 0.001 % |
Otro | 0.002 % Show Supplier Material materials with Otro of 0.002 % |
Silicona | 0.0074 % Show Supplier Material materials with Silicona of 0.0074 % |
Titanio | 0.0001 % Show Supplier Material materials with Titanio of 0.0001 % |
Vanadio | 0.0015 % Show Supplier Material materials with Vanadio of 0.0015 % |
Zinc | 0.001 % Show Supplier Material materials with Zinc of 0.001 % |
Technological properties
Property | ||
---|---|---|
Application areas | High Purity Aluminum / Dilution metal / Capacitor foil / Current collectors / Additive manufacturing / 3D printing / Specilaty alloys / Powder / Sapphire / Battery (Li-ion, Al-Air) | |
Delivery condtion | Available delivery forms: | |
Other | Listed chemical properties represent typical values obtained by Nature Alu. Purity adjustments can be made to meet customer needs on a case-by-case basis. |