Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 99.991 % Show Supplier Material materials with Aluminio of 99.991 % | min. |
Cobre | 1e-05 % Show Supplier Material materials with Cobre of 1e-05 % | Less than |
Cromo | 0.0005 % Show Supplier Material materials with Cromo of 0.0005 % | |
Galio | 0.002 % Show Supplier Material materials with Galio of 0.002 % | |
Hierro | 3e-05 % Show Supplier Material materials with Hierro of 3e-05 % | Less than |
Magnesio | 0.0001 % Show Supplier Material materials with Magnesio of 0.0001 % | |
Manganeso | 0.001 % Show Supplier Material materials with Manganeso of 0.001 % | |
Níquel | 0.0001 % Show Supplier Material materials with Níquel of 0.0001 % | |
Otro | 0.0005 % Show Supplier Material materials with Otro of 0.0005 % | |
Silicona | 0.002 % Show Supplier Material materials with Silicona of 0.002 % | |
Titanio | 0.0001 % Show Supplier Material materials with Titanio of 0.0001 % | |
Vanadio | 0.001 % Show Supplier Material materials with Vanadio of 0.001 % | |
Zinc | 0.001 % Show Supplier Material materials with Zinc of 0.001 % |
Technological properties
Property | ||
---|---|---|
Application areas | High Purity Aluminum / Capacitor foil / Current collectors / Additive manufacturing / 3D printing / Specilaty alloys / Powder / Sapphire / Battery (Li-ion, Al-Air) | |
Delivery condtion | Available delivery forms: | |
Other | Listed chemical properties represent typical values obtained by Nature Alu. Purity adjustments can be made to meet customer needs on a case-by-case basis. The comment "Less than" means that the value is under the OES limit of detection. |