General
Property | Value |
---|---|
Densidad | 8.8 g/cm³ Show Supplier Material materials with Densidad of 8.8 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Strip thickness 0.08 - 3.0 mm, other gauges on request. Strip width from 8.5 mm. Electroplated and Hot-dip tinned strip available. |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.33 [-] | ||
Dureza Vickers | 150 - 205 [-] Show Supplier Material materials with Dureza Vickers of 150 - 205 [-] | R475(1/2H) | For reference only | |
170 - 210 [-] Show Supplier Material materials with Dureza Vickers of 170 - 210 [-] | R550(3/4H) | For reference only | ||
185 - 235 [-] Show Supplier Material materials with Dureza Vickers of 185 - 235 [-] | R585(H) | For reference only | ||
210 - 260 [-] Show Supplier Material materials with Dureza Vickers of 210 - 260 [-] | R670(EH) | For reference only | ||
230 - 270 [-] Show Supplier Material materials with Dureza Vickers of 230 - 270 [-] | R725(SH) | For reference only | ||
245 - 285 [-] Show Supplier Material materials with Dureza Vickers of 245 - 285 [-] | R760(ESH) | For reference only | ||
Elongación | 2 % Show Supplier Material materials with Elongación of 2 % | min. | R760(ESH), A50 | |
3 % Show Supplier Material materials with Elongación of 3 % | min. | R725(SH), A50 | ||
10 % Show Supplier Material materials with Elongación of 10 % | min. | R670(EH), A50 | ||
12 % Show Supplier Material materials with Elongación of 12 % | min. | R585(H), A50 | ||
18 % Show Supplier Material materials with Elongación of 18 % | min. | R550(3/4H), A50 | ||
25 % Show Supplier Material materials with Elongación of 25 % | min. | R475(1/2H), A50 | ||
Límite elástico | 350 MPa Show Supplier Material materials with Límite elástico of 350 MPa | min. | R475(1/2H) | |
485 MPa Show Supplier Material materials with Límite elástico of 485 MPa | min. | R550(3/4H) | ||
540 MPa Show Supplier Material materials with Límite elástico of 540 MPa | min. | R585(H) | ||
635 MPa Show Supplier Material materials with Límite elástico of 635 MPa | min. | R670(EH) | ||
690 MPa Show Supplier Material materials with Límite elástico of 690 MPa | min. | R725(SH) | ||
725 MPa Show Supplier Material materials with Límite elástico of 725 MPa | min. | R760(ESH) | ||
Módulo elástico | 115 GPa Show Supplier Material materials with Módulo elástico of 115 GPa | ||
Plegabilidad 180 ° bidireccional | 0 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 0 [-] | ASTM B820 | R475(1/2H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm |
1 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 1 [-] | ASTM B820 | R550(3/4H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
2 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 2 [-] | ASTM B820 | R585(H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
4 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 4 [-] | ASTM B820 | R670(EH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
7 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 7 [-] | ASTM B820 | R725(SH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
8 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 8 [-] | ASTM B820 | R760(ESH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
Plegabilidad 180 ° en peso bruto | 0 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 0 [-] | ASTM B820 | R475(1/2H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm |
0.5 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 0.5 [-] | ASTM B820 | R550(3/4H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
1 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 1 [-] | ASTM B820 | R585(H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
2 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 2 [-] | ASTM B820 | R670(EH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
5 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 5 [-] | ASTM B820 | R725(SH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
6 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 6 [-] | ASTM B820 | R760(ESH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
Plegabilidad 90 ° bidireccional | 0 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 0 [-] | EN ISO 7438 | R475(1/2H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm |
0.5 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 0.5 [-] | EN ISO 7438 | R550(3/4H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
1 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 1 [-] | EN ISO 7438 | R585(H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
2 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 2 [-] | EN ISO 7438 | R670(EH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
4 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 4 [-] | EN ISO 7438 | R725(SH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
6 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 6 [-] | EN ISO 7438 | R760(ESH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
Plegabilidad 90 ° en peso bruto | 0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | EN ISO 7438 | R475(1/2H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm |
0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | EN ISO 7438 | R550(3/4H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | EN ISO 7438 | R585(H) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
1.5 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 1.5 [-] | EN ISO 7438 | R670(EH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
2.5 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 2.5 [-] | EN ISO 7438 | R725(SH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
4 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 4 [-] | EN ISO 7438 | R760(ESH) | bending thickness: ≤ 0.5 mm & bending width: 10 mm | |
Resistencia a la tracción | 475 - 580 MPa Show Supplier Material materials with Resistencia a la tracción of 475 - 580 MPa | R475(1/2H) | |
550 - 635 MPa Show Supplier Material materials with Resistencia a la tracción of 550 - 635 MPa | R550(3/4H) | ||
585 - 690 MPa Show Supplier Material materials with Resistencia a la tracción of 585 - 690 MPa | R585(H) | ||
670 - 770 MPa Show Supplier Material materials with Resistencia a la tracción of 670 - 770 MPa | R670(EH) | ||
725 - 820 MPa Show Supplier Material materials with Resistencia a la tracción of 725 - 820 MPa | R725(SH) | ||
760 - 840 MPa Show Supplier Material materials with Resistencia a la tracción of 760 - 840 MPa | R760(ESH) |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 377 J/(kg·K) Show Supplier Material materials with Calor específico of 377 J/(kg·K) | ||
Coeficiente de dilatación térmica | 1.82e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.82e-05 1/K | average value between 20-300°C | |
Conductividad térmica | 20 °C | 67 W/(m·K) Show Supplier Material materials with Conductividad térmica of 67 W/(m·K) |
Eléctrico
Chemical properties
Property | Value |
---|---|
Cobre | Balance |
Estaño | 8 % Show Supplier Material materials with Estaño of 8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Application target: Ideal for BTB connector, audio jack and other miniaturized connectors | |
Chemical composition | The chemical composition is the nominal composition of the alloy | |
Coating | Electroplating: Very good Hot dip tinning: Very good | |
Cold Forming | Very good | |
Machining | Not suitable | |
Packaging size | Standard coils with outside diameters up to 1300 mm. Traverse-wound coils with drum weights up to 500 kg. Multiple-coil up to 3 tons. | |
Soldering general | Soft soldering: Good | |
Testings | Fatigue strength: The fatigue strength is defined as the maximum bending stress amplitude which a material withstands for 10.000.000 load cycles under symmetrical alternate load without breaking. It depends on the temper selected and can be estimated typically by 1/3 of tensile strength. For solid solution fine grain materials fatigue strength might increase up to 0,5 * of tensile strength. Bending test: 90° bend test According to EN ISO 7438, 180° bend test acc. to ASTM B820, shown values might show orange- peel, however no crack. | |
Welding | Laser welding: Good Resistance welding: Good |