General
Property | Value |
---|---|
Densidad | 8.93 g/cm³ Show Supplier Material materials with Densidad of 8.93 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Strip thickness 0.08 - 3.0 mm, other gauges on request. Strip width from 8.5 mm. Electroplated and Hot-dip tinned strip available. |
Mecánica
Property | Value | Testing Standard | Comment |
---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.33 [-] | ||
Dureza Vickers | 110 - 130 [-] Show Supplier Material materials with Dureza Vickers of 110 - 130 [-] | R360 | For reference only | |
120 - 150 [-] Show Supplier Material materials with Dureza Vickers of 120 - 150 [-] | R420 | For reference only | ||
130 [-] Show Supplier Material materials with Dureza Vickers of 130 [-] | min. | R460 | For reference only | ||
Elongación | 2 % Show Supplier Material materials with Elongación of 2 % | min. | R420, A50 | |
3 % Show Supplier Material materials with Elongación of 3 % | min. | R360, A50 | ||
Límite elástico | 300 MPa Show Supplier Material materials with Límite elástico of 300 MPa | min. | R360 | |
350 MPa Show Supplier Material materials with Límite elástico of 350 MPa | min. | R420 | ||
410 MPa Show Supplier Material materials with Límite elástico of 410 MPa | min. | R460 | ||
Módulo elástico | 120 GPa Show Supplier Material materials with Módulo elástico of 120 GPa | ||
Plegabilidad 180 ° bidireccional | 1 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 1 [-] | ASTM B820 | R360 | bending thickness ≤ 0.5 mm & bending width: 10 mm |
2.5 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 2.5 [-] | ASTM B820 | R420 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
4 [-] Show Supplier Material materials with Plegabilidad 180 ° bidireccional of 4 [-] | ASTM B820 | R460 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
Plegabilidad 180 ° en peso bruto | 1 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 1 [-] | ASTM B820 | R360 | bending thickness ≤ 0.5 mm & bending width: 10 mm |
2 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 2 [-] | ASTM B820 | R420 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
2.5 [-] Show Supplier Material materials with Plegabilidad 180 ° en peso bruto of 2.5 [-] | ASTM B820 | R460 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
Plegabilidad 90 ° bidireccional | 0 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 0 [-] | EN ISO 7438 | R360 | bending thickness ≤ 0.5 mm & bending width: 10 mm |
1 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 1 [-] | EN ISO 7438 | R420 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
2 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 2 [-] | EN ISO 7438 | R460 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
Plegabilidad 90 ° en peso bruto | 0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | EN ISO 7438 | R360 | bending thickness ≤ 0.5 mm & bending width: 10 mm |
1 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 1 [-] | EN ISO 7438 | R420 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
1.5 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 1.5 [-] | EN ISO 7438 | R460 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
Resistencia a la tracción | 360 - 430 MPa Show Supplier Material materials with Resistencia a la tracción of 360 - 430 MPa | R360 | |
420 - 490 MPa Show Supplier Material materials with Resistencia a la tracción of 420 - 490 MPa | R420 |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 385 J/(kg·K) Show Supplier Material materials with Calor específico of 385 J/(kg·K) | ||
Coeficiente de dilatación térmica | 1.73e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.73e-05 1/K | average value between 20-300°C | |
Conductividad térmica | 20 °C | 330 W/(m·K) Show Supplier Material materials with Conductividad térmica of 330 W/(m·K) |
Eléctrico
Chemical properties
Property | Value |
---|---|
Cobre | Balance |
Estaño | 0.15 % Show Supplier Material materials with Estaño of 0.15 % |
Technological properties
Property | ||
---|---|---|
Application areas | Application target: Ideal for power connectors. | |
Chemical composition | The chemical composition is the nominal composition of the alloy | |
Coating | Electroplating: Good Hot dip tinning: Good | |
Cold Forming | Good | |
Machining | Not suitable | |
Packaging size | Standard coils with outside diameters up to 1300 mm. Traverse-wound coils with drum weights up to 500 kg. Multiple-coil up to 3 tons. | |
Soldering general | Soft soldering: Good | |
Testings | Fatigue strength: The fatigue strength is defined as the maximum bending stress amplitude which a material withstands for 10.000.000 load cycles under symmetrical alternate load without breaking. It depends on the temper selected and can be estimated typically by 1/3 of tensile strength. For solid solution fine grain materials fatigue strength might increase up to 0,5 * of tensile strength. Bending test: 90° bend test According to EN ISO 7438, 180° bend test acc. to ASTM B820, shown values might show orange- peel, however no crack. | |
Welding | Laser welding: Good Resistance welding: Good |