General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.82 g/cm³ Show Supplier Material materials with Densidad of 7.82 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 1350 - 2540 mm Show Supplier Material materials with Ancho of 1350 - 2540 mm |
Diámetro exterior | 450 - 910 mm Show Supplier Material materials with Diámetro exterior of 450 - 910 mm |
Diámetro interior | 400 - 730 mm Show Supplier Material materials with Diámetro interior of 400 - 730 mm |
Espesor | 150 - 230 mm Show Supplier Material materials with Espesor of 150 - 230 mm |
Longitud | 1750 - 3370 mm Show Supplier Material materials with Longitud of 1750 - 3370 mm |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.035 % Show Supplier Material materials with Azufre of 0 - 0.035 % |
Carbono | 0.36 - 0.44 % Show Supplier Material materials with Carbono of 0.36 - 0.44 % |
Cobre | 0 - 0.3 % Show Supplier Material materials with Cobre of 0 - 0.3 % |
Cromo | 0.8 - 1.1 % Show Supplier Material materials with Cromo of 0.8 - 1.1 % |
Fósforo | 0 - 0.04 % Show Supplier Material materials with Fósforo of 0 - 0.04 % |
Hierro | Balance |
Manganeso | 0.5 - 0.8 % Show Supplier Material materials with Manganeso of 0.5 - 0.8 % |
Níquel | 0 - 0.3 % Show Supplier Material materials with Níquel of 0 - 0.3 % |
Silicona | 0.17 - 0.37 % Show Supplier Material materials with Silicona of 0.17 - 0.37 % |
Technological properties
Property | ||
---|---|---|
Application areas | Instrumental steel for milling cutter, mining equipment, etc., Die steel for glass making, plastic making and for automobile industry, Roller-bearing steel, Shaft steel, steel for turbines and generators, heat-resistant alloy for aerospace industry and for power turbine, Nickel alloys for chemical industry, Cold-rolled steel, High nytrogen steel | |
Processing methods | Method of electroclag remelting (ESR). |