General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.7 g/cm³ Show Supplier Material materials with Densidad of 2.7 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Ancho | 1943 mm Show Supplier Material materials with Ancho of 1943 mm | max. |
Espesor | 6.35 - 101.6 mm Show Supplier Material materials with Espesor of 6.35 - 101.6 mm | |
Longitud | 8990 mm Show Supplier Material materials with Longitud of 8990 mm | max. |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 28 % Show Supplier Material materials with Elongación of 28 % |
Límite elástico | 23.0 °C | 28 MPa Show Supplier Material materials with Límite elástico of 28 MPa |
Módulo elástico | 23.0 °C | 68.9 GPa Show Supplier Material materials with Módulo elástico of 68.9 GPa |
Resistencia a la tracción | 23.0 °C | 83 MPa Show Supplier Material materials with Resistencia a la tracción of 83 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.38E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.38E-5 1/K | for 23-100°C |
Conductividad térmica | 23.0 °C | 234 W/(m·K) Show Supplier Material materials with Conductividad térmica of 234 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 3.57E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 3.57E+7 S/m |
Specific Electrical conductivity | 61.5 % IACS Show Supplier Material materials with Specific Electrical conductivity of 61.5 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Boro | 6E-3 % Show Supplier Material materials with Boro of 6E-3 % | max. | |
Cobre | 0.01 % Show Supplier Material materials with Cobre of 0.01 % | max. | |
Cromo | 3E-3 % Show Supplier Material materials with Cromo of 3E-3 % | max. | |
Galio | 0.02 % Show Supplier Material materials with Galio of 0.02 % | max. | |
Hierro | 0.1 - 0.18 % Show Supplier Material materials with Hierro of 0.1 - 0.18 % | ||
Magnesio | 0.01 % Show Supplier Material materials with Magnesio of 0.01 % | max | |
Manganeso | 3E-3 % Show Supplier Material materials with Manganeso of 3E-3 % | max. | |
Silicona | 0.07 % Show Supplier Material materials with Silicona of 0.07 % | max. | |
Titanio | 4E-3 % Show Supplier Material materials with Titanio of 4E-3 % | max., Ti+V | |
Vanadio | 4E-3 % Show Supplier Material materials with Vanadio of 4E-3 % | max. | |
Zinc | 0.03 % Show Supplier Material materials with Zinc of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | This product is especially suitable for electrical applications. It is used for bus bar manufacturing that specializes in the transport and the distribution of electricity. PCP Aluminium developed this product to meet complex electrical requirements in order to minimize energy loss. This product is available in a variety of sizes. | |
Availability | Other thicknesses, widhts and lengths may be available upon inquiry. On request, this product may be milled and coated with protective plastic film on the milled sides. | |
Dimensional stability | Excellent | |
Other | AA1370 is the best aluminium you can get for electrical applications: It is made of prime metal without any recycled alloying material. AA1370 is a subset of AA1350 aluminium. 99.7% pure aluminium ensures increased conductivity. PCP aluminium AA1370-50 is annealed (0) since it becomes less prone to deformation with a stress relief heat treatment. | |
Processing history | Fabricated from prime aluminium cast ingots | |
Welding | Excellent weldability |