General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2.66 g/cm³ Show Supplier Material materials with Densidad of 2.66 g/cm³ | |
Rugosidad superficial | 25.4 μm Show Supplier Material materials with Rugosidad superficial of 25.4 μm | max. |
Medidas
Property | Value | Comment |
---|---|---|
Ancho | 2591 mm Show Supplier Material materials with Ancho of 2591 mm | max. |
Espesor | 6.35 - 101.6 mm Show Supplier Material materials with Espesor of 6.35 - 101.6 mm | |
Longitud | 8990 mm Show Supplier Material materials with Longitud of 8990 mm | max. |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 70 [-] Show Supplier Material materials with Dureza Brinell of 70 [-] |
Elongación | 23.0 °C | 16 % Show Supplier Material materials with Elongación of 16 % |
Límite elástico | 23.0 °C | 124 MPa Show Supplier Material materials with Límite elástico of 124 MPa |
Módulo elástico | 23.0 °C | 71 GPa Show Supplier Material materials with Módulo elástico of 71 GPa |
Resistencia a la tracción | 23.0 °C | 283 MPa Show Supplier Material materials with Resistencia a la tracción of 283 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.38E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.38E-5 1/K | for 23-100°C |
Conductividad térmica | 23.0 °C | 120 W/(m·K) Show Supplier Material materials with Conductividad térmica of 120 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.57E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.57E+7 S/m |
Specific Electrical conductivity | 27 % IACS Show Supplier Material materials with Specific Electrical conductivity of 27 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Circonio | 0.15 % Show Supplier Material materials with Circonio of 0.15 % | max., Zr+Ti | |
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % | max. | |
Cromo | 0.05 - 0.25 % Show Supplier Material materials with Cromo of 0.05 - 0.25 % | ||
Hierro | 0.4 % Show Supplier Material materials with Hierro of 0.4 % | max. | |
Magnesio | 4 - 4.9 % Show Supplier Material materials with Magnesio of 4 - 4.9 % | ||
Manganeso | 0.4 - 1 % Show Supplier Material materials with Manganeso of 0.4 - 1 % | ||
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | max. | |
Titanio | 0.15 % Show Supplier Material materials with Titanio of 0.15 % | max., Zr+Ti | |
Zinc | 0.25 % Show Supplier Material materials with Zinc of 0.25 % | max. |
Technological properties
Property | ||
---|---|---|
Anodizing | Hard anodizing: Excellent; Decorative: Not suitable | |
Application areas | Robotic component, Rubber & Plastic mold, Vacuum chamber, Prototyping, Jig, Template | |
Availability | MAX5® mold products are available in temper O3 (homogenized) aluminum in the following size: | |
Corrosion properties | Inland atmosphere: Excellent; Marine atmosphere: Good | |
Dimensional stability | Excellent | |
General machinability | Excellent | |
Polishing ability | Very good | |
Welding | WIG/MIG: very good; By resistance: very good |