General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 18.75 - 18.85 g/cm³ Show Supplier Material materials with Densidad of 18.75 - 18.85 g/cm³ |
Rugosidad superficial | 1 μm Show Supplier Material materials with Rugosidad superficial of 1 μm |
Medidas
Property | Value |
---|---|
Diámetro | 3.5 - 20 mm Show Supplier Material materials with Diámetro of 3.5 - 20 mm |
Longitud | 300 - 1600 mm Show Supplier Material materials with Longitud of 300 - 1600 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 3.5 x 500-1524; 4.5 x 500-1524; 5.5 x 500-1524; 6.5 x 500-1524; 7 x 500-1524; 7.5 x 500-1524; 8.5 x 500-1524; 12.7 x 300-1524; 20 x 300-1600 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 30 | 23.0 °C | 400 - 420 [-] Show Supplier Material materials with Dureza Vickers 30 of 400 - 420 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % | ||
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % | ||
Carbono | 6E-4 % Show Supplier Material materials with Carbono of 6E-4 % | ||
Cobre | 1E-4 % Show Supplier Material materials with Cobre of 1E-4 % | ||
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % | ||
Hierro | 8E-4 % Show Supplier Material materials with Hierro of 8E-4 % | ||
Lantano | 0.77 - 0.94 % Show Supplier Material materials with Lantano of 0.77 - 0.94 % | as La | |
Molibdeno | 1.2E-3 % Show Supplier Material materials with Molibdeno of 1.2E-3 % | ||
Nitrógeno | 1E-4 % Show Supplier Material materials with Nitrógeno of 1E-4 % | ||
Níquel | 2E-4 % Show Supplier Material materials with Níquel of 2E-4 % | ||
Otro | 0.9 - 1.1 % Show Supplier Material materials with Otro of 0.9 - 1.1 % | as La₂O₃ | |
Plomo | 1E-4 % Show Supplier Material materials with Plomo of 1E-4 % | ||
Potasio | 1E-4 % Show Supplier Material materials with Potasio of 1E-4 % | ||
Silicona | 1E-4 % Show Supplier Material materials with Silicona of 1E-4 % | ||
Wolframio | balance |
Technological properties
Property | ||
---|---|---|
Application areas | WL is a popular choice for ion sources, lamp electrodes and welding electrodes. |