General
Property | Temperature | Value |
---|---|---|
Sección transversal de captura neutrónica | 23.0 °C | 0 m² Show Supplier Material materials with Sección transversal de captura neutrónica of 0 m² |
Densidad | 23.0 °C | 19.1 g/cm³ Show Supplier Material materials with Densidad of 19.1 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 30 - 80 mm Show Supplier Material materials with Diámetro of 30 - 80 mm |
Longitud | 100 - 2000 mm Show Supplier Material materials with Longitud of 100 - 2000 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 30 x 300-1800; 35 x 300-1800; 40 x 300-3000; 45 x 300-2400; 50 x 300-1900; 70 x 100-2200; 80 x 100-2000 |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 30 | 23.0 °C | 350 - 460 [-] Show Supplier Material materials with Dureza Vickers 30 of 350 - 460 [-] |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 3420 °C Show Supplier Material materials with Temperatura de fusión of 3420 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Función de trabajo | 23.0 °C | 4.54 eV Show Supplier Material materials with Función de trabajo of 4.54 eV |
Acústico
Chemical properties
Property | Value |
---|---|
Aluminio | 1E-4 % Show Supplier Material materials with Aluminio of 1E-4 % |
Cadmio | 1E-4 % Show Supplier Material materials with Cadmio of 1E-4 % |
Carbono | 6E-4 % Show Supplier Material materials with Carbono of 6E-4 % |
Cobre | 1E-4 % Show Supplier Material materials with Cobre of 1E-4 % |
Cromo | 3E-4 % Show Supplier Material materials with Cromo of 3E-4 % |
Hierro | 8E-4 % Show Supplier Material materials with Hierro of 8E-4 % |
Molibdeno | 1.2E-3 % Show Supplier Material materials with Molibdeno of 1.2E-3 % |
Nitrógeno | 1E-4 % Show Supplier Material materials with Nitrógeno of 1E-4 % |
Níquel | 2E-4 % Show Supplier Material materials with Níquel of 2E-4 % |
Oxígeno | 2E-4 % Show Supplier Material materials with Oxígeno of 2E-4 % |
Plomo | 1E-4 % Show Supplier Material materials with Plomo of 1E-4 % |
Potasio | 1E-4 % Show Supplier Material materials with Potasio of 1E-4 % |
Silicona | 1E-4 % Show Supplier Material materials with Silicona of 1E-4 % |
Wolframio | 99.97 % Show Supplier Material materials with Wolframio of 99.97 % |
Technological properties
Property | ||
---|---|---|
Application areas | Tungsten rods are mainly used in the lighting industry and high temperature furnace construction. |