General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua, equilibrio | 23.0 °C | 0.3 % Show Supplier Material materials with Absorción de agua, equilibrio of 0.3 % | max., ASTM D4442 |
Densidad | 23.0 °C | 1.07 g/cm³ Show Supplier Material materials with Densidad of 1.07 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 72 [-] Show Supplier Material materials with Dureza Shore D of 72 [-] | ASTM D2240 |
Elongación | 23.0 °C | 70 % Show Supplier Material materials with Elongación of 70 % | min., ASTM D638 |
Impact strength, Izod notched, ASTM | -30.0 °C | 160 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 160 J/m | min., ASTM D256 |
23.0 °C | 850 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 850 J/m | min., ASTM D256 | |
Módulo de flexión | 23.0 °C | 1.6 GPa Show Supplier Material materials with Módulo de flexión of 1.6 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 70 MPa Show Supplier Material materials with Resistencia a la flexión of 70 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 43 MPa Show Supplier Material materials with Resistencia a la tracción of 43 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 50 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 50 °C | ASTM D648 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.6 - 2 % Show Supplier Material materials with Contracción of 1.6 - 2 % | ASTM D955 |
Velocidad de flujo de la masa derretida | 15 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 15 g/10min | min., ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | Electromechanical parts and accessories, Hardware, Baby Strollers, Office furniture, Tent bracket, Suitcase accessories, Sports equipment, Medical Equipment-Hospital Bed Caster, Sporting Goods-Roller Skate Plate, Suitcase wheels | |
Color | Natural |