General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 115 [-] Show Supplier Material materials with Hardness, Rockwell R of 115 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 90 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 3.73 GPa Show Supplier Material materials with Módulo de flexión of 3.73 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 100 MPa Show Supplier Material materials with Resistencia a la flexión of 100 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 - 1 % Show Supplier Material materials with Contracción of 0.3 - 1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Baby Strollers, Bicycle brake parts, Bicycle, Snow shoe, Skates, Leisure sports equipment, Power tool housing, Skate sole, Wheelchair wheel frame. | |
Color | Black | |
Fillers | 15% Glass Fiber |