General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua, equilibrio | 23.0 °C | 0.3 % Show Supplier Material materials with Absorción de agua, equilibrio of 0.3 % | max., ASTM D4442 |
Densidad | 23.0 °C | 1.14 g/cm³ Show Supplier Material materials with Densidad of 1.14 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 78 [-] Show Supplier Material materials with Dureza Shore D of 78 [-] | ASTM D2240 |
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % | min., ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 50 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 2.7 GPa Show Supplier Material materials with Módulo de flexión of 2.7 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 110 MPa Show Supplier Material materials with Resistencia a la flexión of 110 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 67 MPa Show Supplier Material materials with Resistencia a la tracción of 67 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.2 - 1.6 % Show Supplier Material materials with Contracción of 1.2 - 1.6 % | ASTM D955 |
Velocidad de flujo de la masa derretida | 80 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 80 g/10min | min., ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | Buckle pull ring, Baby Strollers, Electrical and electronic parts, Information technology equipment parts, Tool housing, Sports equipment, Bicycles-Chain Cover, Gear, Automobiles parts. | |
Color | Black |