General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 90 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 7.7 GPa Show Supplier Material materials with Módulo de flexión of 7.7 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 230 MPa Show Supplier Material materials with Resistencia a la flexión of 230 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 155 MPa Show Supplier Material materials with Resistencia a la tracción of 155 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 - 0.6 % Show Supplier Material materials with Contracción of 0.2 - 0.6 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Office chairs-Chair base and Armrest, Electrical and Pneumatic Hand Tools-Pneumatic tool housing | |
Color | Black | |
Fillers | 35% Glass Fiber |