General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 11 GPa Show Supplier Material materials with Módulo de flexión of 11 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 290 MPa Show Supplier Material materials with Resistencia a la flexión of 290 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 - 0.4 % Show Supplier Material materials with Contracción of 0.1 - 0.4 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Sports equipment, Power tool housing, Hand tool, Bicycle brake parts, Fishing tackle reel, Scroll door, Office desk & chair, Home appliance parts, Motor housing, Hairdryer nozzle, Baby storllers-Buckle axle | |
Color | Black | |
Fillers | 45% Glass Fiber |