General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 110 [-] Show Supplier Material materials with Hardness, Rockwell R of 110 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 3.8 GPa Show Supplier Material materials with Módulo de flexión of 3.8 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 130 MPa Show Supplier Material materials with Resistencia a la flexión of 130 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 - 0.8 % Show Supplier Material materials with Contracción of 0.2 - 0.8 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical and Pneumatic Hand Tools- Anti-Static handle | |
Color | Natural |