General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 100 [-] Show Supplier Material materials with Hardness, Rockwell R of 100 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 140 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 140 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 3.4 GPa Show Supplier Material materials with Módulo de flexión of 3.4 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 120 MPa Show Supplier Material materials with Resistencia a la flexión of 120 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 73 MPa Show Supplier Material materials with Resistencia a la tracción of 73 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 - 1 % Show Supplier Material materials with Contracción of 0.3 - 1 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Electromechanical parts and accessories, Hardware, Mechanical parts, Snowshoe, Skates, Leisure sports equipment, Baby Stroller-Stroller axle-Stroller handrail bracket-Stroller hinge bracket-Stroller wheel fork, Sporting Goods-Water bottle cages, Medical equipment-Medical shoe accessories | |
Color | Black | |
Fillers | 15% Glass Fiber |