General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua, equilibrio | 23.0 °C | 0.3 % Show Supplier Material materials with Absorción de agua, equilibrio of 0.3 % | max., ASTM D4442 |
Densidad | 23.0 °C | 1.17 g/cm³ Show Supplier Material materials with Densidad of 1.17 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 77 [-] Show Supplier Material materials with Dureza Shore D of 77 [-] | ASTM D2240 |
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | max., ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 30 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 30 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 3.2 GPa Show Supplier Material materials with Módulo de flexión of 3.2 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 130 MPa Show Supplier Material materials with Resistencia a la flexión of 130 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | UL 94 (1.6mm) V0 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.7 - 0.9 % Show Supplier Material materials with Contracción of 0.7 - 0.9 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Connector, Electrical switch housing, Cooling Fan, Power tools, Machine tool motor housing, Industrial Parts & Components-Thread Spool | |
Color | Natural |