General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua, equilibrio | 23.0 °C | 0.3 % Show Supplier Material materials with Absorción de agua, equilibrio of 0.3 % | max., ASTM D4442 |
Densidad | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Densidad of 1.38 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 140 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 140 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 8.82 GPa Show Supplier Material materials with Módulo de flexión of 8.82 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 280 MPa Show Supplier Material materials with Resistencia a la flexión of 280 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 180 MPa Show Supplier Material materials with Resistencia a la tracción of 180 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 - 0.4 % Show Supplier Material materials with Contracción of 0.2 - 0.4 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Kitchenware and utensils, Home appliances. Electromechanical parts and accessories, Hardware, Mechanical parts. Switch, Breaker, Motor parts, Office Chair Base, Office Chair Caster, Office furniture. Sports equipment, Plug, Fan blades, Plastic screw, Gear, Nut. Industrial Parts & Components-Industrial Thread Spool, Automobiles-Cooling Fan | |
Color | Natural | |
Fillers | 33% Glass Fiber |