General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua, equilibrio | 23.0 °C | 0.3 % Show Supplier Material materials with Absorción de agua, equilibrio of 0.3 % | max., ASTM D4442 |
Densidad | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Densidad of 1.38 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 90 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 8.33 GPa Show Supplier Material materials with Módulo de flexión of 8.33 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 250 MPa Show Supplier Material materials with Resistencia a la flexión of 250 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 135 MPa Show Supplier Material materials with Resistencia a la tracción of 135 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 - 0.4 % Show Supplier Material materials with Contracción of 0.2 - 0.4 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Air filter housing, Automobiles curtain, Automobiles gear assembly, Automobiles-Rearview mirror Rotation Axes. Home appliances. Scooters-Scooters Exhaust Heat Shield. Electromechanical parts and accessories, Harware, Mechanical parts. Office Chair Base, Office Chair Caster, Office furniture. Sports equipment, Plug, Fan blades, Plastic screw, Gear, Bicycle brake disc, Nut. | |
Color | Black | |
Fillers | 33% Glass Fiber |