General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua, equilibrio | 23.0 °C | 0.3 % Show Supplier Material materials with Absorción de agua, equilibrio of 0.3 % | max., ASTM D4442 |
Densidad | 23.0 °C | 1.14 g/cm³ Show Supplier Material materials with Densidad of 1.14 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 80 [-] Show Supplier Material materials with Dureza Shore D of 80 [-] | ASTM D2240 |
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % | min., ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 50 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 2.8 GPa Show Supplier Material materials with Módulo de flexión of 2.8 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 120 MPa Show Supplier Material materials with Resistencia a la flexión of 120 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 68 MPa Show Supplier Material materials with Resistencia a la tracción of 68 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.2 - 1.6 % Show Supplier Material materials with Contracción of 1.2 - 1.6 % | ASTM D955 |
Velocidad de flujo de la masa derretida | 70 - 250 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 70 - 250 g/10min | ASTM D1238 |
Technological properties
Property | ||
---|---|---|
Application areas | Washer, Baby Strollers, Electrical and electronic parts, Information technology equipment parts, Tool housing , Sports equipment, Gear, Sporting goods-Glasses temples Automobiles parts | |
Color | Black |