General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua, equilibrio | 23.0 °C | 0.3 % Show Supplier Material materials with Absorción de agua, equilibrio of 0.3 % | max., ASTM D4442 |
Densidad | 23.0 °C | 1.55 g/cm³ Show Supplier Material materials with Densidad of 1.55 g/cm³ | ASTM D792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 170 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 170 J/m | ASTM D256 |
Módulo de flexión | 23.0 °C | 13.73 GPa Show Supplier Material materials with Módulo de flexión of 13.73 GPa | ASTM D790 |
Resistencia a la flexión | 23.0 °C | 355 MPa Show Supplier Material materials with Resistencia a la flexión of 355 MPa | ASTM D790 |
Resistencia a la tracción | 23.0 °C | 210 MPa Show Supplier Material materials with Resistencia a la tracción of 210 MPa | ASTM D638 |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 - 0.4 % Show Supplier Material materials with Contracción of 0.2 - 0.4 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Buckle, Electromechanical parts and accessories, Hardware, Machanical parts. Sports equipment, Plug, Fan blades, Plastic screw, Gear, Bicycle brake disc, Nut. | |
Color | Natural | |
Fillers | 50% Glass Fiber |