Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 500 J/(kg·K) Show Supplier Material materials with Calor específico of 500 J/(kg·K) |
Difusividad térmica | 20.0 °C | 199 mm²/s Show Supplier Material materials with Difusividad térmica of 199 mm²/s |
Temperatura de fusión | 1440 °C Show Supplier Material materials with Temperatura de fusión of 1440 °C |
General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Supplier Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 166 [-] Show Supplier Material materials with Dureza Brinell of 166 [-] |
Elongación | 20.0 °C | 45 % Show Supplier Material materials with Elongación of 45 % |
Límite elástico | 20.0 °C | 260 MPa Show Supplier Material materials with Límite elástico of 260 MPa |
Módulo elástico | 20.0 °C | 199 GPa Show Supplier Material materials with Módulo elástico of 199 GPa |
Resistencia a la tracción | 20.0 °C | 550 MPa Show Supplier Material materials with Resistencia a la tracción of 550 MPa |
Chemical properties
Property | Value |
---|---|
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cobre | 3 - 4 % Show Supplier Material materials with Cobre of 3 - 4 % |
Cromo | 16 - 18 % Show Supplier Material materials with Cromo of 16 - 18 % |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |
Níquel | 7 - 9 % Show Supplier Material materials with Níquel of 7 - 9 % |
Silicona | 0.6 % Show Supplier Material materials with Silicona of 0.6 % |
Technological properties
Property | ||
---|---|---|
Application areas | fashion lifestyle, kitchen cookware, tableware, healthcare, hospital eqiupment, toolong trolley, medical, public saniitation:toilet, handrail and button, outdoor bottles, automotive interior | |
Processing history | Annealing |