General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.11 g/cm³ Show Supplier Material materials with Densidad of 1.11 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.11 [-] Show Supplier Material materials with Densidad relativa of 1.11 [-] | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % | ISO 527 | break, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 157 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 157 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 48 J Show Supplier Material materials with Instrumented Impact, Total Energy of 48 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 2.6 GPa Show Supplier Material materials with Módulo de flexión of 2.6 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.6 GPa Show Supplier Material materials with Módulo elástico of 2.6 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 108 MPa Show Supplier Material materials with Resistencia a la flexión of 108 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 51 MPa Show Supplier Material materials with Resistencia a la tracción of 51 MPa | ISO 527 | break, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 14 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8.2E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 8.2E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 875 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 875 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature, 1.80 MPa | 101 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 101 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 95 °C Show Supplier Material materials with Relative temperature index, electrical of 95 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 95 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 95 °C | UL 746B | |||
Temperatura de flexión bajo carga | 101 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 101 °C | ||||
Temperatura de reblandecimiento Vicat | 120 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 120 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101362812- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UV-light, water exposure/immersion: F2- UL 746C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 4 |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Supplier Material materials with Índice de seguimiento comparativo of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 25.4 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 25.4 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Velocidad de flujo del volumen derretido | 32 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 32 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Energy Management | |
Availability | Europe,Asia,MEA,Americas | |
Processing methods | Drying Temperature: 95 to 100.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |