Polyamide 66 (PA66)
Zytel® 70G43L NC010Polyamide 66 (PA66)
RADIFLAM A RV250 AF 375 BKSuministrada por:
RadiciGroup High Performance PolymersPolyamide 6 (PA6)
Zytel® 73G30HSL NC010Polyamide 66 (PA66)
Zytel® 70G43HSLA BK099Polyamide 66 (PA66)
RADILON A RV350HHR 3800 BKSuministrada por:
RadiciGroup High Performance PolymersTereftalato de polibutileno (PBT)
RADITER B ERV300TKB 3827 BKSuministrada por:
RadiciGroup High Performance Polymers