General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.15 % Show Supplier Material materials with Absorción de agua of 0.15 % | ASTM D 570 | (23°C/24hrs) |
Densidad | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Densidad of 1.19 g/cm³ | ASTM D 792 |
Densidad relativa | 23.0 °C | 1.2 [-] Show Supplier Material materials with Densidad relativa of 1.2 [-] | ASTM D 792 | |
Specific volume | 23.0 °C | 0.83 cm³/g Show Supplier Material materials with Specific volume of 0.83 cm³/g | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dureza Rockwell M | 23.0 °C | 70 [-] Show Supplier Material materials with Dureza Rockwell M of 70 [-] | ASTM D 785 | | ||
Elongación | 23.0 °C | 6 % Show Supplier Material materials with Elongación of 6 % | ISO 527 | yield, 50 mm/min | ||
Hardness, Rockwell R | 23.0 °C | 118 [-] Show Supplier Material materials with Hardness, Rockwell R of 118 [-] | ASTM D 785 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 801 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 801 J/m | ASTM D 256 | notched, 23°C | ||
Impact strength, Izod unnotched, ASTM | 23.0 °C | 3204 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 3204 J/m | ASTM D 4812 | 23°C | ||
Instrumented Impact, at Peak | 23.0 °C | 63 J Show Supplier Material materials with Instrumented Impact, at Peak of 63 J | ASTM D 3763 | 23°C | ||
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | ISO 527 | 1 mm/min | ||
Resistencia a la flexión | 23.0 °C | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | ISO 178 | yield, 2 mm/min | ||
Resistencia a la tracción | 23.0 °C | 63 MPa Show Supplier Material materials with Resistencia a la tracción of 63 MPa | ISO 527 | yield, 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 35 kJ/m² | ISO 179/2C | 23°C | ||
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 12 kJ/m² | ISO 180/1A | 80*10*4, 23°C | ||
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | ASTM D 1044 | CS-17, 1 kg | ||
Resistencia al choque, ensayo Charpy no entallado | ISO 179/1eU | Unnotch Edgew 80*10*4 sp=62mm, -30°C | ||||
Resistencia al choque, ensayo Izod no entallado | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |
Calor específico | 23.0 °C | 1.25E-3 J/(kg·K) Show Supplier Material materials with Calor específico of 1.25E-3 J/(kg·K) | ASTM C 351 |
Coeficiente de dilatación térmica | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C |
Conductividad térmica | 23.0 °C | 0.2 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.2 W/(m·K) | ISO 8302 |
Heat deflection temperature, 0.45 MPa | 136 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 136 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Heat deflection temperature, 1.80 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 125 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Temperatura de flexión bajo carga | 125 - 136 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 125 - 136 °C | ||
Temperatura de reblandecimiento Vicat | 142 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 142 °C | ISO 306 | Rate B/120 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.96 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.96 [-] | ASTM D 150 |
Dielectric constant, 60Hz | 23.0 °C | 3.17 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3.17 [-] | ASTM D 150 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.01 [-] | ASTM D 150 | |
Dissipation factor, 50Hz | 23.0 °C | 9E-4 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 9E-4 [-] | ASTM D 150 | 50/60 Hz |
Rigidez dieléctrica | 23.0 °C | 14.9 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 14.9 kV/mm | ASTM D 149 | in air, 3.2 mm |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | >, ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 10.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 10.5 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Velocidad de flujo del volumen derretido | 10 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 10 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, Pharmaceutical Packaging & Drug Delivery | |
Availability | Europe,Asia,MEA,Americas,Global | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |