General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.07 % Show Supplier Material materials with Absorción de agua of 0.07 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.35 g/cm³ Show Supplier Material materials with Densidad of 1.35 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.6 % Show Supplier Material materials with Elongación of 2.6 % | ISO 527 | break, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 147 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 147 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 650 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 650 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 20 J Show Supplier Material materials with Instrumented Impact, at Peak of 20 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 6.3 GPa Show Supplier Material materials with Módulo de flexión of 6.3 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 6.8 GPa Show Supplier Material materials with Módulo elástico of 6.8 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 166 MPa Show Supplier Material materials with Resistencia a la flexión of 166 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 112 MPa Show Supplier Material materials with Resistencia a la tracción of 112 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 147 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 147 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.5E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Heat deflection temperature, 0.45 MPa | 121 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 121 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 115 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 115 °C | ASTM D 648 | 3.2mm, unannealed | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de flexión bajo carga | 115 - 121 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 115 - 121 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104088917- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=104123741- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.3mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥1.5mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3.27 [-] Show Supplier Material materials with Constante dieléctrica of 3.27 [-] | SABIC method | 1.9 GHz |
Dielectric constant, 10GHz | 23.0 °C | 3.28 [-] Show Supplier Material materials with Dielectric constant, 10GHz of 3.28 [-] | SABIC method |
Dielectric constant, 1GHz | 23.0 °C | 3.24 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 3.24 [-] | SABIC method | 1.1 GHz |
Dielectric constant, 5GHz | 23.0 °C | 3.28 [-] Show Supplier Material materials with Dielectric constant, 5GHz of 3.28 [-] | SABIC method |
Dissipation factor, 1GHz | 23.0 °C | 6.6E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 6.6E-3 [-] | SABIC method | |
Dissipation factor, 5GHz | 23.0 °C | 7.1E-3 [-] Show Supplier Material materials with Dissipation factor, 5GHz of 7.1E-3 [-] | SABIC method |
Factor de disipación | 23.0 °C | 6.7E-3 [-] Show Supplier Material materials with Factor de disipación of 6.7E-3 [-] | SABIC method |
Índice de seguimiento comparativo | 23.0 °C | 175 V Show Supplier Material materials with Índice de seguimiento comparativo of 175 V | IEC 60112 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | ASTM D 955 | 24 hrs |
Contracción transversal | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción transversal of 0.2 % | ASTM D 955 | 24 hrs |
Velocidad de flujo de la masa derretida | 12 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 12 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Velocidad de flujo del volumen derretido | 20 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 20 cm³/10min | ISO 1133 | MVR at 300°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Data Transfer, Audio, Watch/Jewelry, Wireless Communications, Personal Computing | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |