Resistencia al choque, ensayo Charpy entallado: 14 kJ/m²

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar® 740

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 740 RED

Suministrada por:

Arkema: High Performance Polymers

Policarbonato (PC)

LEXAN™ Copolymer FXE141R

Suministrada por:

Sabic

Polyamide 46 (PA46)

Stanyl® 46HF5040

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE250F9

Suministrada por:

DSM Engineering Materials

Policarbonato (PC)

LNP™ THERMOCOMP™ Compound D251

Suministrada por:

Sabic

Polyamide 46 (PA46)

Stanyl® TS250F8

Suministrada por:

DSM Engineering Materials

Éter de polifenileno (PPE)

NORYL™ Resin V0150B - Asia

Suministrada por:

Sabic

Éter de polifenileno (PPE)

NORYL™ Resin V0150B - Americas

Suministrada por:

Sabic

Polyamide 46 (PA46)

Stanyl® TW200F8

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-G6

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F10

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 80G33HS1L NC010

Polyamide 46 (PA46)

Stanyl® TW241F8

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-HG7

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Zytel® 73G30L NC010

Polyamide 46 (PA46)

Stanyl® TE200F8

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-G8

Suministrada por:

DSM Engineering Materials

Polioximetileno (POM)

Delrin® 100P NC010
Página 1 de 10