General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.35 % Show Supplier Material materials with Absorción de agua of 0.35 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Densidad of 1.19 g/cm³ | ASTM D 792 |
Densidad relativa | 23.0 °C | 1.2 [-] Show Supplier Material materials with Densidad relativa of 1.2 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | ISO 62 | (23°C / 50% RH) |
Specific volume | 23.0 °C | 0.83 cm³/g Show Supplier Material materials with Specific volume of 0.83 cm³/g | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dureza Rockwell M | 23.0 °C | 70 [-] Show Supplier Material materials with Dureza Rockwell M of 70 [-] | ASTM D 785 | | ||
Elongación | 23.0 °C | 6 % Show Supplier Material materials with Elongación of 6 % | ISO 527 | yield, 50 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 95 MPa Show Supplier Material materials with Hardness, Ball Indentation of 95 MPa | ISO 2039-1 | H358/30 | ||
Hardness, Rockwell R | 23.0 °C | 118 [-] Show Supplier Material materials with Hardness, Rockwell R of 118 [-] | ASTM D 785 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 801 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 801 J/m | ASTM D 256 | notched, 23°C | ||
Impact strength, Izod unnotched, ASTM | 23.0 °C | 3204 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 3204 J/m | ASTM D 4812 | 23°C | ||
Instrumented Impact, Total Energy | 23.0 °C | 70 J Show Supplier Material materials with Instrumented Impact, Total Energy of 70 J | ASTM D 3763 | 23°C | ||
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | ISO 527 | 1 mm/min | ||
Resistencia a la flexión | 23.0 °C | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | ISO 178 | yield, 2 mm/min | ||
Resistencia a la tracción | 23.0 °C | 63 MPa Show Supplier Material materials with Resistencia a la tracción of 63 MPa | ISO 527 | yield, 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C | ||
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 12 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C | ||
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | ASTM D 1044 | CS-17, 1 kg | ||
Resistencia al choque, ensayo Charpy no entallado | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, 23°C | ||||
Resistencia al choque, ensayo Izod no entallado | ISO 180/1U | 80*10*3, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Calor específico | 23.0 °C | 1.25E-3 J/(kg·K) Show Supplier Material materials with Calor específico of 1.25E-3 J/(kg·K) | ASTM C 351 | ||
Coeficiente de dilatación térmica | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Conductividad térmica | 23.0 °C | 0.2 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.2 W/(m·K) | ISO 8302 | ||
Heat deflection temperature, 0.45 MPa | 136 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 136 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 125 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Temperatura de flexión bajo carga | 125 - 136 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 125 - 136 °C | ||||
Temperatura de reblandecimiento Vicat | 142 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 142 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228425- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.7mm UL 94 <br> UV-light, water exposure/immersion: F2- UL 746C <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=541348- - <br> UL Yellow Card Link 3: https://iq.ul.com/ul/cert.aspx?ULID=220939- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.96 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.96 [-] | ASTM D 150 |
Dielectric constant, 60Hz | 23.0 °C | 3.17 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3.17 [-] | ASTM D 150 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.01 [-] | ASTM D 150 | |
Dissipation factor, 50Hz | 23.0 °C | 9E-4 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 9E-4 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.1 mm Show Supplier Material materials with Hot-Wire Ignition of 1.1 mm | ≥, UL 746A | PLC 3 |
Rigidez dieléctrica | 23.0 °C | 14.9 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 14.9 kV/mm | ASTM D 149 | in air, 3.2 mm |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | >, ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Supplier Material materials with Índice de seguimiento comparativo of 3 V | UL 746A | (UL) {PLC} |
Óptico
Property | Value | Comment |
---|---|---|
Transmission | 88 % Show Supplier Material materials with Transmission of 88 % | ASTM D 1003 | 2.54 mm |
Turbidez | 1 % Show Supplier Material materials with Turbidez of 1 % | ASTM D 1003 | 2.54 mm |
Índice de refracción | 1.59 [-] Show Supplier Material materials with Índice de refracción of 1.59 [-] | ASTM D542 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 10.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 10.5 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Velocidad de flujo del volumen derretido | 11 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 11 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosure/Housing/Cover, Individual Equiptment, Forward Lighting, Building Accessory, Cluster, Data Transfer, Document Handling, LED Lighting, Rear/Signal Lighting, Wireless Communications, Irrigation | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |