General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.03 [-] Show Supplier Material materials with Densidad relativa of 1.03 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 63 [-] Show Supplier Material materials with Dureza Shore D of 63 [-] | ASTM D 2240 | 10S reading |
Elongación | 23.0 °C | 50 % Show Supplier Material materials with Elongación of 50 % | ISO 527 | break, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 560 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 560 J/m | ASTM D 256 |
Módulo de flexión | 23.0 °C | 0.8 GPa Show Supplier Material materials with Módulo de flexión of 0.8 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 0.7 GPa Show Supplier Material materials with Módulo elástico of 0.7 GPa | ISO 527 | 1 mm/min |
Resistencia a la tracción | 23.0 °C | 25 MPa Show Supplier Material materials with Resistencia a la tracción of 25 MPa | ISO 527 | break, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 37 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 37 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 82 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 82 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 66 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 66 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Temperatura de flexión bajo carga | 66 - 82 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 66 - 82 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 2.47 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.47 [-] | ASTM D 150 |
Dissipation factor, 1GHz | 23.0 °C | 3.2E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 3.2E-3 [-] | ASTM D 150 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 33 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 33 g/10min | ASTM D 1238 | 280°C/5.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Airbag, Auto Electrical, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |