Módulo de flexión: 0.8 GPa

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3120-50

Suministrada por:

Arkema: High Performance Polymers

Polyamide 46 (PA46)

Stanyl® TW341

Suministrada por:

DSM Engineering Materials

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3121-50

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3120-10

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3120-15

Suministrada por:

Arkema: High Performance Polymers

Polyamide 46 (PA46)

Stanyl® TW341-FC

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE300

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW341-N

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE341

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TS341

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TS300

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW341-J

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW441-FC

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW441

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW341-B

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® HGR3-W (P1120D)

Suministrada por:

DSM Engineering Materials

Polietileno de alta densidad (PEAD)

PE METALEN PE-11K

Suministrada por:

JSC METACLAY

Polietileno lineal de baja densidad

G-3938 (LLDPE)

Suministrada por:

GREENAGE INDUSTRIES

Polietileno (PE)

LNP™ LUBRICOMP™ Compound FL004 - Asia

Suministrada por:

Sabic