General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | ASTM D 570 | (23°C/48hrs) |
Densidad relativa | 23.0 °C | 1.03 [-] Show Supplier Material materials with Densidad relativa of 1.03 [-] | ASTM D 792 |
Índice límite de óxigeno | 23.0 °C | 25 % Show Supplier Material materials with Índice límite de óxigeno of 25 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 56 [-] Show Supplier Material materials with Dureza Shore D of 56 [-] | ISO 868 |
Elongación | 23.0 °C | 90 % Show Supplier Material materials with Elongación of 90 % | ISO 527 | break, 50 mm/min |
Módulo de flexión | 23.0 °C | 0.7 GPa Show Supplier Material materials with Módulo de flexión of 0.7 GPa | ISO 178 | 12.5 mm/min |
Resistencia a la tracción | 23.0 °C | 23 MPa Show Supplier Material materials with Resistencia a la tracción of 23 MPa | ISO 527 | break, 50 mm/min |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Brittleness temperature | -40 °C Show Supplier Material materials with Brittleness temperature of -40 °C | <, ASTM D 746 | |
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 3.0 mm | |
Heat deflection temperature, 0.45 MPa | 85 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 85 °C | ASTM D 648 | 6.4 mm, unannealed | |
Temperatura de flexión bajo carga | 85 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 85 °C | ||
Temperatura de reblandecimiento Vicat | 102 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 102 °C | ISO 306 | Rate A/50 | |
Inflamabilidad | Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Smoke Density on 0.5mm plaque, Flame, Ds, max: 150- ASTM E 662 <br> Smoke Density on 0.5mm plaque, Non-flame, Ds, max: 75- ASTM E 662 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.5 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.5 [-] | IEC 60250 |
Dielectric constant, 60Hz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.6 [-] | IEC 60250 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 3.8E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 3.8E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 0.02 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 0.02 [-] | IEC 60250 | 50/60 Hz |
Rigidez dieléctrica | 23.0 °C | 26 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 26 kV/mm | IEC 60243-1 | in oil, 2.0mm |
Volume resistivity | 23.0 °C | 3.90E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 3.90E+16 Ω·cm | IEC 60093 |
Índice de seguimiento comparativo | 23.0 °C | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | IEC 60112 | |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 5.1 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 5.1 g/10min | ASTM D 1238 | 250°C/10.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Data Transfer, Wire & cable | |
Availability | Americas | |
Processing methods | Screen Pack: 150 to 100.0- | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |