Polyvinylidenefluoride (PVDF)
Kynar Superflex® 2500-20Suministrada por:
Arkema: High Performance PolymersCopoliéster termoplástico
Hytrel® G5544Copoliéster termoplástico
Hytrel® 5553FG NC010Polyvinylidenefluoride (PVDF)
Kynar Superflex® 2500-25Suministrada por:
Arkema: High Performance PolymersPolibuteno
Poly(butene-1) PBCopoliéster termoplástico
Hytrel® HTR8441 BK316Polytetrafluoroethylene (PTFE)
3M™ Dyneon™ (PTFE Granules TF 1620)Polytetrafluoroethylene (PTFE)
3M™ Dyneon™ (PTFE Granules TF 1641)Polytetrafluoroethylene (PTFE)
3M™ Dyneon™ (PTFE Granules TF 1645)Polytetrafluoroethylene (PTFE)
3M™ Dyneon™ (PTFE Powder TF 1750)