General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.18 % Show Supplier Material materials with Absorción de agua of 0.18 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.11 g/cm³ Show Supplier Material materials with Densidad of 1.11 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.11 [-] Show Supplier Material materials with Densidad relativa of 1.11 [-] | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | ISO 62 | (23°C / 50% RH) |
Índice límite de óxigeno | 23.0 °C | 32 % Show Supplier Material materials with Índice límite de óxigeno of 32 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % | ISO 527 | break, 50 mm/min |
Hardness, Ball Indentation | 23.0 °C | 113 MPa Show Supplier Material materials with Hardness, Ball Indentation of 113 MPa | ISO 2039-1 | H358/30 |
Impact strength, Izod notched, ASTM | 23.0 °C | 330 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 330 J/m | ASTM D 256 |
Instrumented Impact, Total Energy | 23.0 °C | 50 J Show Supplier Material materials with Instrumented Impact, Total Energy of 50 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 110 MPa Show Supplier Material materials with Resistencia a la flexión of 110 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 70 MPa Show Supplier Material materials with Resistencia a la tracción of 70 MPa | ISO 527 | yield, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 14 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 13 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Taber Abrasion | 23.0 °C | 35 mg/1000cy Show Supplier Material materials with Taber Abrasion of 35 mg/1000cy | SABIC method | CS-17, 1 kg |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball pressure temperature | 140 °C Show Supplier Material materials with Ball pressure temperature of 140 °C | IEC 60695-10-2 | approximate maximum | |||
Coeficiente de dilatación térmica | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 9E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 9E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Conductividad térmica | 23.0 °C | 0.27 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.27 W/(m·K) | ISO 8302 | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature, 0.45 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 140 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 130 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 130 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 115 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 115 °C | UL 746B | |||
Temperatura de flexión bajo carga | 130 - 140 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 130 - 140 °C | ||||
Temperatura de reblandecimiento Vicat | 155 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 155 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94-5VA Flame Class Rating: ≥2mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 775°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.5 mm: 775°C IEC 60695-2-13 <br> UL Recognized, 94V-1 Flame Class Rating: ≥0.8mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=599099- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=100146076- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.7 [-] | IEC 60250 |
Dielectric constant, 60Hz | 23.0 °C | 2.8 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.8 [-] | IEC 60250 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 3E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 3E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 9E-4 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 9E-4 [-] | IEC 60250 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 0.8 mm Show Supplier Material materials with High Amp Arc Ignition of 0.8 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0.8 mm Show Supplier Material materials with Hot-Wire Ignition of 0.8 mm | ≥, UL 746A | PLC 0 |
Rigidez dieléctrica | 23.0 °C | 16 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 16 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 | |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Supplier Material materials with Índice de seguimiento comparativo of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 3.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 3.5 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Velocidad de flujo del volumen derretido | 10 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 10 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Pump, Photovoltaic Components, Plumbing, Non-LED Lighting, Personal Computing, Infrastructure, Medical Device, LED Lighting, Washing Machine, Wiring Devices, Wireless Communications, Coffee Maker/Espresso Machine, Document Handling, Dishwasher, Circuit Protection, Amusement Machine, Enclosure/Housing/Cover, Electronics, Energy Management, Enclosures, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 300 to 320.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |